Online PCB Manufacturing poor tin defects analysis and solutions
Online PCB manufacturing defect reason analysis
1. Component leads and pads are poorly solderable and difficult to tin on.
2. Flux activity is low, and the oxide layer on the leads and pads cannot be completely removed.
3. The solder pot has a low liquid level and the solder does not completely cover the pad.
4. The preheating temperature is low, the flux activity is not fully activated, and the oxide layer is not completely removed.
5. Tin pot temperature is low, solder wetting time and temperature are not enough
6. The plate speed is too fast, the solder is too late to fill
Solutions
1.During Online PCB manufacturing, using a slightly more active flux or increasing the amount of flux used
2. Adjust the immersion tin depth and replenish the solder
3. Adjust the preheating temperature
4. Adjust the temperature of the tin pot
5. Adjust the transmission speed